Specification
Retarder Material | Muscovite Mica |
Beam Deviation | 10 arcsec |
Wavefront | /10 @ 633 nm |
Clear Aperture | 85% of central diameter |
Surface Quality | 40-20 scratch dig |
Retardation Tolerance | /50 for 532 nm type |
Homogeneity of Retardation | /200 |
Diameter Tolerance | +0 / -0.1 mm |
Damage Threshold, pulsed | 10 J/cm, 11 ns, 100 Hz @ 1064 nm |
Damage Threshold, cw | 0.5 kw/cm @ VIS-NIR |
Temperature Coefficient of Retardation per C | negligible |
Standard Retardations | /4, /2 |